Paintspecification - Hempel​

​Preparation

Fully assembled container shall be automatically abrasive blasted to SA 2 ½ according to Swedish standard SIS 05 05900. The blast profile to be in accordance with Bn9a shall be apprx. 50 microns. Particular attention shall be paied to the under frame in the shot blasting booth. The container shall be lifted to enable access to the under frame. All metal preparation shall be carried out just prior to assembly. Dry film thickness shall be established on accordance with with ISO 2808, DS/R 454, SSPC-PA 2 and DIN 55928 Teil 2.

Paint-System

Hempel A/S, 2800 Lyngby, Denmark

Exterior:​

Primer:

HEMPADUR PRIMER 1536 two component epoxy zinc rich primer.

dry film thickness 40 microns

Topcoat

HEMPATEX 4641 - RAL Code to be advised

dry film thickness 80 microns

total minimum dry film thickness 120 microns

Interior:

​Primer

HEMPADUR PRIMER 1536 two component epoxy zinc rich primer.

dry film thickness 30 microns

Topcoat

HEMPADUR HB 4522 two component, high build epoxy paint - RAL code to be advised

dry film thickness 50 microns

total minimum dry film thickness 80 microns

Underframe:

​Primer

HEMPADUR PRIMER 15300-19830 two component polyamide cured zinc phosphate solvent primer.

dry film thickness 40 microns

Finish coat

HEMPINOL 10220-19990

dry film thickness 175 microns

total minimum dry film thickness 215 microns

The dry film thickness specified is minimum. ​

Har du spørgsmål? Ring til os på +45 7027 6780 eller skriv til mail@ijcu.dk  -   Køb, salg og udlejning i høj kvalitet  -  Landsdækkende udlejning - Virksomhed med mange års erfaring

​Vi kontakter dig inden for en halv time

 
 
Nogle felter er ikke udfyldt korrekt

IJ-Container ApS

CVR: 10926181​ 

Kongelysvej 6B

DK-2820 Gentofte (Copenhagen)

Tlf. +45 70 27 67 80

E-mail: mail@ijcu.dk